QUICK METHOD FOR BOND WORK INDEXAPPROXIMATE …
micrometers in size. According to the Bond standard procedure, the work index is determined by simulating a dry grinding in a closed circuit in the Bond ball mill to achieve 250% circulating load (Bond, 1949, 1952, 1961). The test is performed on a raw material approximately weighing 10 kg, which coarseness is -3.327 mm.