Flotation technology of refractory low-grade …
The rough molybdenum concentrate could be obtained by three-minute flotation with grinding fineness of −0.074 mm accounting for 80%, sodium carbonate dosage of 1500 g/t, sodium silicate dosage of 1500 g/t, kerosene dosage …